As-deposited, half-stack As-deposited, full-stack Annealed, half-stack Annealed, full-stack Annealed, full-stack Fig 4.3 Ratio of the 1550nm peak to the 980nm peak (at V40) for ZnS:ErF3 half and full stack devices in the as deposited or annealed conditions.